Nickel Alloy9 compared properties
PropertyHaynes 214Haynes 242Difference
Yield strength577 MPa845 MPa+46%
Tensile strength975 MPa1,290 MPa+32%
Elongation37.3 %33.7 %-10%
Elastic modulus218,000 MPa229,000 MPa+5%
Poisson ratio0.30.30%
Density8,050 kg/m³9,050 kg/m³+12%
Thermal conductivity12 W/m·K11.3 W/m·K-6%
Coefficient of thermal expansion0.000013 1/K0.000011 1/K-17%
Melting point1,378 °C1,333 °C-3%

Difference is Haynes 242 relative to Haynes 214. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Haynes 214
grade
214
standard
Haynes International Datasheet H-3008
heat treatment
Annealed
Haynes 242
grade
242
standard
Haynes International Datasheet H-3079
heat treatment
Aged