Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/ATI N-90 vs Haynes 242

ATI N-90 vs Haynes 242

Property comparison of ATI N-90 and Haynes 242, both nickel alloy.

Nickel Alloy4 compared properties
PropertyATI N-90Haynes 242Difference
Yield strength695 MPa845 MPa+22%
Tensile strength1,080 MPa1,290 MPa+19%
Elongation20 %33.7 %+69%
Density8,110 kg/m³9,050 kg/m³+12%

Difference is Haynes 242 relative to ATI N-90. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI N-90
grade
Ni-Cr-Co (N07090)
standard
BS 2HR2
heat treatment
Aged (bar)
Haynes 242
grade
242
standard
Haynes International Datasheet H-3079
heat treatment
Aged

What else is in Engineering Database

Related comparisons

View each material