PropertyHaynes 230Haynes 242Difference
Yield strength390 MPa845 MPa+117%
Tensile strength860 MPa1,290 MPa+50%
Elongation47.7 %33.7 %-29%
Elastic modulus211,000 MPa229,000 MPa+9%
Poisson ratio0.310.3-3%
Density9,050 kg/m³9,050 kg/m³0%
Thermal conductivity8.9 W/m·K11.3 W/m·K+27%
Specific heat397 J/kg·K386 J/kg·K-3%
Coefficient of thermal expansion0.000013 1/K0.000011 1/K-15%
Melting point1,333 °C1,333 °C0%

Difference is Haynes 242 relative to Haynes 230. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Haynes 230
grade
230
standard
Haynes International Datasheet H-3000
heat treatment
Annealed
Haynes 242
grade
242
standard
Haynes International Datasheet H-3079
heat treatment
Aged

What else is in Engineering Database

Related comparisons

View each material