Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/Haynes 214 vs Haynes 282

Haynes 214 vs Haynes 282

Property comparison of Haynes 214 and Haynes 282, both nickel alloy.

Nickel Alloy9 compared properties
PropertyHaynes 214Haynes 282Difference
Yield strength577 MPa384 MPa-33%
Tensile strength975 MPa839 MPa-14%
Elongation37.3 %59 %+58%
Elastic modulus218,000 MPa217,000 MPa0%
Poisson ratio0.30.30%
Density8,050 kg/m³8,270 kg/m³+3%
Thermal conductivity12 W/m·K10.3 W/m·K-14%
Coefficient of thermal expansion0.000013 1/K0.000012 1/K-7%
Melting point1,378 °C1,338 °C-3%

Difference is Haynes 282 relative to Haynes 214. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Haynes 214
grade
214
standard
Haynes International Datasheet H-3008
heat treatment
Annealed
Haynes 282
grade
282
standard
Haynes International Datasheet H-3173
heat treatment
Annealed