Haynes 214 vs Haynes 282
Property comparison of Haynes 214 and Haynes 282, both nickel alloy.
| Property | Haynes 214 | Haynes 282 | Difference |
|---|---|---|---|
| Yield strength | 577 MPa | 699 MPa | +21% |
| Tensile strength | 975 MPa | 1,132 MPa | +16% |
| Elongation | 37.3 % | 33 % | -12% |
| Elastic modulus | 218,000 MPa | 217,000 MPa | 0% |
| Poisson ratio | 0.3 | 0.3 | 0% |
| Density | 8,050 kg/m³ | 8,290 kg/m³ | +3% |
| Thermal conductivity | 12 W/m·K | 10.3 W/m·K | -14% |
| Coefficient of thermal expansion | 0.000013 1/K | 0.000012 1/K | -7% |
| Melting point | 1,378 °C | 1,338 °C | -3% |
Difference is Haynes 282 relative to Haynes 214. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
Haynes 214
- grade
- 214
- standard
- Haynes International Datasheet H-3008
- heat treatment
- Annealed
Haynes 282
- grade
- 282
- standard
- Haynes International Datasheet H-3173
- heat treatment
- Aged (Solution Annealed + Double Aged)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators