Home/Compare/Tin Alloy/Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Property comparison of Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base and Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base, both tin alloy.

Tin Alloy5 compared properties
PropertyBabbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-baseBabbitt Grade 7 (Pb-9.3Sn-15Sb) lead-baseDifference
Tensile strength71 MPa72 MPa+1%
Density10,000 kg/m³10,000 kg/m³0%
Brinell hardness21 HB22.5 HB+7%
Coefficient of thermal expansion0.000026 1/K0.000026 1/K0%
Melting point265 °C254 °C-4%

Difference is Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base relative to Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base
grade
Grade 15 lead-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base
grade
Grade 7 lead-base
standard
ASTM B23
heat treatment
chill cast