Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Tin Alloy/Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base vs Babbitt Grade 2 (Sn-7.5Sb-3.5Cu) tin-base

Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base vs Babbitt Grade 2 (Sn-7.5Sb-3.5Cu) tin-base

Property comparison of Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base and Babbitt Grade 2 (Sn-7.5Sb-3.5Cu) tin-base, both tin alloy.

Tin Alloy6 compared properties
PropertyBabbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-baseBabbitt Grade 2 (Sn-7.5Sb-3.5Cu) tin-baseDifference
Tensile strength71 MPa77 MPa+8%
Elastic modulus23,000 MPa52,000 MPa+126%
Density10,000 kg/m³7,390 kg/m³-26%
Brinell hardness21 HB24.5 HB+17%
Coefficient of thermal expansion0.000026 1/K0.000022 1/K-15%
Melting point265 °C298 °C+12%

Difference is Babbitt Grade 2 (Sn-7.5Sb-3.5Cu) tin-base relative to Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base
grade
Grade 15 lead-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 2 (Sn-7.5Sb-3.5Cu) tin-base
grade
Grade 2 tin-base
standard
ASTM B23
heat treatment
chill cast