Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Tin Alloy/Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Property comparison of Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base and Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base, both tin alloy.

Tin Alloy7 compared properties
PropertyBabbitt Grade 13 (Pb-6Sn-10Sb) lead-baseBabbitt Grade 7 (Pb-9.3Sn-15Sb) lead-baseDifference
Yield strength23 MPa24 MPa+4%
Tensile strength70 MPa72 MPa+3%
Elongation5 %4 %-20%
Density10,200 kg/m³10,000 kg/m³-2%
Brinell hardness19 HB22.5 HB+18%
Coefficient of thermal expansion0.000026 1/K0.000026 1/K0%
Melting point249 °C254 °C+2%

Difference is Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base relative to Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base
grade
Grade 13 lead-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base
grade
Grade 7 lead-base
standard
ASTM B23
heat treatment
chill cast