Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Tin Alloy/Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Property comparison of Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base and Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base, both tin alloy.

Tin Alloy7 compared properties
PropertyBabbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-baseBabbitt Grade 7 (Pb-9.3Sn-15Sb) lead-baseDifference
Yield strength30 MPa24 MPa-20%
Tensile strength64 MPa72 MPa+13%
Elongation2 %4 %+100%
Density7,340 kg/m³10,000 kg/m³+36%
Brinell hardness17 HB22.5 HB+32%
Coefficient of thermal expansion0.000021 1/K0.000026 1/K+24%
Melting point297 °C254 °C-14%

Difference is Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base relative to Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base
grade
Grade 1 tin-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base
grade
Grade 7 lead-base
standard
ASTM B23
heat treatment
chill cast