Tin Alloy6 compared properties
PropertyBabbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-baseBabbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-baseDifference
Tensile strength64 MPa71 MPa+11%
Elastic modulus50,000 MPa23,000 MPa-54%
Density7,340 kg/m³10,000 kg/m³+36%
Brinell hardness17 HB21 HB+24%
Coefficient of thermal expansion0.000021 1/K0.000026 1/K+24%
Melting point297 °C265 °C-11%

Difference is Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base relative to Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 1 (Sn-4.5Sb-4.5Cu) tin-base
grade
Grade 1 tin-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base
grade
Grade 15 lead-base
standard
ASTM B23
heat treatment
chill cast