Home/Compare/Tin Alloy/Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base vs Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base

Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base vs Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base

Property comparison of Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base and Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base, both tin alloy.

Tin Alloy5 compared properties
PropertyBabbitt Grade 13 (Pb-6Sn-10Sb) lead-baseBabbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-baseDifference
Tensile strength70 MPa71 MPa+1%
Density10,200 kg/m³10,000 kg/m³-2%
Brinell hardness19 HB21 HB+11%
Coefficient of thermal expansion0.000026 1/K0.000026 1/K0%
Melting point249 °C265 °C+6%

Difference is Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base relative to Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base
grade
Grade 13 lead-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 15 (Pb-1Sn-16Sb-1As) lead-base
grade
Grade 15 lead-base
standard
ASTM B23
heat treatment
chill cast