ATI N-90 vs ATI W-722
Property comparison of ATI N-90 and ATI W-722, both nickel alloy.
| Property | ATI N-90 | ATI W-722 | Difference |
|---|---|---|---|
| Yield strength | 695 MPa | 655 MPa | -6% |
| Tensile strength | 1,080 MPa | 1,000 MPa | -7% |
| Elongation | 20 % | 15 % | -25% |
| Density | 8,110 kg/m³ | 8,320 kg/m³ | +3% |
Difference is ATI W-722 relative to ATI N-90. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
ATI N-90
- grade
- Ni-Cr-Co (N07090)
- standard
- BS 2HR2
- heat treatment
- Aged (bar)
ATI W-722
- grade
- Ni-Cr-Fe-Ti (N07722)
- standard
- UNS N07722
- heat treatment
- Aged (bar)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators