Minimum preheat and maximum interpass temperatures for welding per AWS D1.1, ASME BPVC, ASME B31.3, and EN 1011. Covers carbon steels (AWS categories A/B), HSLA (category C, HPS 70W/100W), quenched and tempered (category D), Cr-Mo alloys (P5/P11/P22/P91/P4/P5B), austenitic stainless (P8), duplex stainless (P10H), nickel alloys, aluminum, titanium, and copper. Each record includes base metal group, thickness range, carbon equivalent, preheat/interpass temperatures in both F and C, PWHT requirements, hydrogen control level, and welding process notes. 46 records.

Civil Engineeringbase_metal_group: nickel_alloy1 row
base metal groupAWS group numberPWHT requiredbase metal exampleshydrogen controlinterpass max C (degC)interpass max F (degF)preheat min C (degC)preheat min F (degF)record keythickness range inthickness range mmwelding process notes
nickel_alloyF-No.41-45noAlloy 625 / Alloy 825 / Alloy 276; Inconel / Incoloy gradeslow_H2_required1503002170F-No.41-45#anyanyanyPreheat to room temperature minimum (70°F); clean base metal thoroughly; max interpass 300°F; use matching filler (ERNiCrMo-3 for 625); avoid contamination from Cu or Pb

This is a sample. Search the full welding preheat interpass dataset and 300+ more by creating a free account and accessing the database.

Get started for FREE

Related data