Welding Preheat Interpass
Minimum preheat and maximum interpass temperatures for welding per AWS D1.1, ASME BPVC, ASME B31.3, and EN 1011. Covers carbon steels (AWS categories A/B), HSLA (category C, HPS 70W/100W), quenched and tempered (category D), Cr-Mo alloys (P5/P11/P22/P91/P4/P5B), austenitic stainless (P8), duplex stainless (P10H), nickel alloys, aluminum, titanium, and copper. Each record includes base metal group, thickness range, carbon equivalent, preheat/interpass temperatures in both F and C, PWHT requirements, hydrogen control level, and welding process notes. 46 records.
Attributes
AWS_group_number
base_metal_examples
thickness_range_in
thickness_range_mm
carbon_equivalent_CE_max
preheat_min_FdegF
preheat_min_CdegC
interpass_max_FdegF
interpass_max_CdegC
PWHT_required
PWHT_temp_range_F
hydrogen_control
welding_process_notes
Browse data
Search the full welding preheat interpass dataset with natural language or structured queries.
Search this table