Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Refractory/Rhenium (Re pure >99.9%) vs Ta-2.5W (Ta-97.5-W-2.5) annealed

Rhenium (Re pure >99.9%) vs Ta-2.5W (Ta-97.5-W-2.5) annealed

Property comparison of Rhenium (Re pure >99.9%) and Ta-2.5W (Ta-97.5-W-2.5) annealed, both refractory.

Refractory4 compared properties
PropertyRhenium (Re pure >99.9%)Ta-2.5W (Ta-97.5-W-2.5) annealedDifference
Elastic modulus463,000 MPa186,000 MPa-60%
Density21,020 kg/m³16,600 kg/m³-21%
Coefficient of thermal expansion0.000006 1/K0.000006 1/K+3%
Melting point3,186 °C2,996 °C-6%

Difference is Ta-2.5W (Ta-97.5-W-2.5) annealed relative to Rhenium (Re pure >99.9%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Rhenium (Re pure >99.9%)
standard
CRC Handbook of Chemistry and Physics 103rd Ed.
heat treatment
annealed
grade
Ta-2.5W (Ta-97.5-W-2.5) annealed
standard
ASTM B365 R05252 / Plansee Ta alloy product data
heat treatment
annealed
grade
R05252