PropertyRhenium (Re pure >99.9%)Ta-10W (Ta-90-W-10) annealedDifference
Elastic modulus463,000 MPa193,000 MPa-58%
Density21,020 kg/m³16,850 kg/m³-20%
Coefficient of thermal expansion0.000006 1/K0.000006 1/K+3%
Melting point3,186 °C3,080 °C-3%

Difference is Ta-10W (Ta-90-W-10) annealed relative to Rhenium (Re pure >99.9%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Rhenium (Re pure >99.9%)
standard
CRC Handbook of Chemistry and Physics 103rd Ed.
heat treatment
annealed
grade
Ta-10W (Ta-90-W-10) annealed
standard
ASTM B365 R05255 / ATI Ta-10W technical datasheet
heat treatment
annealed
grade
R05255