Home/Compare/Refractory/Silica Refractory Brick (>93% SiO2) vs Ta-2.5W (Ta-97.5-W-2.5) annealed

Silica Refractory Brick (>93% SiO2) vs Ta-2.5W (Ta-97.5-W-2.5) annealed

Property comparison of Silica Refractory Brick (>93% SiO2) and Ta-2.5W (Ta-97.5-W-2.5) annealed, both refractory.

Refractory3 compared properties
PropertySilica Refractory Brick (>93% SiO2)Ta-2.5W (Ta-97.5-W-2.5) annealedDifference
Elastic modulus40,000 MPa186,000 MPa+365%
Density1,900 kg/m³16,600 kg/m³+774%
Coefficient of thermal expansion0.000012 1/K0.000006 1/K-47%

Difference is Ta-2.5W (Ta-97.5-W-2.5) annealed relative to Silica Refractory Brick (>93% SiO2). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Silica Refractory Brick (>93% SiO2)
standard
ASTM
grade
heat treatment
Ta-2.5W (Ta-97.5-W-2.5) annealed
standard
ASTM B365 R05252 / Plansee Ta alloy product data
grade
R05252
heat treatment
annealed