Refractory9 compared properties
PropertyMolybdenum (Mo pure >99.94%)Rhenium (Re pure >99.9%)Difference
Elastic modulus329,000 MPa463,000 MPa+41%
Shear modulus127,000 MPa178,000 MPa+40%
Poisson ratio0.290.3+3%
Density10,220 kg/m³21,020 kg/m³+106%
Brinell hardness160 HB134 HB-16%
Thermal conductivity138 W/m·K48 W/m·K-65%
Specific heat251 J/kg·K137 J/kg·K-45%
Coefficient of thermal expansion0.000005 1/K0.000006 1/K+22%
Melting point2,623 °C3,186 °C+21%

Difference is Rhenium (Re pure >99.9%) relative to Molybdenum (Mo pure >99.94%). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Molybdenum (Mo pure >99.94%)
grade
Mo pure
standard
ASTM
heat treatment
Stress-Relieved
Rhenium (Re pure >99.9%)
grade
standard
CRC Handbook of Chemistry and Physics 103rd Ed.
heat treatment
annealed