Refractory6 compared properties
PropertyNb-1Zr (Nb-99-Zr-1) annealedRhenium (Re pure >99.9%)Difference
Elastic modulus103,000 MPa463,000 MPa+350%
Poisson ratio0.40.3-25%
Density8,590 kg/m³21,020 kg/m³+145%
Thermal conductivity52 W/m·K48 W/m·K-8%
Coefficient of thermal expansion0.000007 1/K0.000006 1/K-15%
Melting point2,399 °C3,186 °C+33%

Difference is Rhenium (Re pure >99.9%) relative to Nb-1Zr (Nb-99-Zr-1) annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Nb-1Zr (Nb-99-Zr-1) annealed
grade
R04251
standard
ASTM B392 Type 3 (R04251) / CRC Handbook
heat treatment
annealed
Rhenium (Re pure >99.9%)
grade
standard
CRC Handbook of Chemistry and Physics 103rd Ed.
heat treatment
annealed