PropertyHaynes 230Haynes 282Difference
Yield strength390 MPa384 MPa-2%
Tensile strength860 MPa839 MPa-2%
Elongation47.7 %59 %+24%
Elastic modulus211,000 MPa217,000 MPa+3%
Poisson ratio0.310.3-3%
Density9,050 kg/m³8,270 kg/m³-9%
Thermal conductivity8.9 W/m·K10.3 W/m·K+16%
Specific heat397 J/kg·K436 J/kg·K+10%
Coefficient of thermal expansion0.000013 1/K0.000012 1/K-5%
Melting point1,333 °C1,338 °C0%

Difference is Haynes 282 relative to Haynes 230. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Haynes 230
grade
230
standard
Haynes International Datasheet H-3000
heat treatment
Annealed
Haynes 282
grade
282
standard
Haynes International Datasheet H-3173
heat treatment
Annealed