Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Tin Alloy/Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base vs Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base

Property comparison of Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base and Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base, both tin alloy.

Tin Alloy7 compared properties
PropertyBabbitt Grade 3 (Sn-8Sb-8Cu) tin-baseBabbitt Grade 7 (Pb-9.3Sn-15Sb) lead-baseDifference
Yield strength45 MPa24 MPa-47%
Tensile strength69 MPa72 MPa+4%
Elongation1 %4 %+300%
Density7,460 kg/m³10,000 kg/m³+34%
Brinell hardness27 HB22.5 HB-17%
Coefficient of thermal expansion0.000022 1/K0.000026 1/K+18%
Melting point331 °C254 °C-23%

Difference is Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base relative to Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base
grade
Grade 3 tin-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base
grade
Grade 7 lead-base
standard
ASTM B23
heat treatment
chill cast

What else is in Engineering Database

Related comparisons

View each material