Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Tin Alloy/Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base vs Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base

Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base vs Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base

Property comparison of Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base and Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base, both tin alloy.

Tin Alloy7 compared properties
PropertyBabbitt Grade 13 (Pb-6Sn-10Sb) lead-baseBabbitt Grade 3 (Sn-8Sb-8Cu) tin-baseDifference
Yield strength23 MPa45 MPa+96%
Tensile strength70 MPa69 MPa-1%
Elongation5 %1 %-80%
Density10,200 kg/m³7,460 kg/m³-27%
Brinell hardness19 HB27 HB+42%
Coefficient of thermal expansion0.000026 1/K0.000022 1/K-15%
Melting point249 °C331 °C+33%

Difference is Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base relative to Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 13 (Pb-6Sn-10Sb) lead-base
grade
Grade 13 lead-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 3 (Sn-8Sb-8Cu) tin-base
grade
Grade 3 tin-base
standard
ASTM B23
heat treatment
chill cast

What else is in Engineering Database

Related comparisons

View each material