| Property | ATI 59 (UNS N06059) | ATI 601 (UNS N06601) | Difference |
|---|---|---|---|
| Yield strength | 310 MPa | 440 MPa | +42% |
| Tensile strength | 690 MPa | 790 MPa | +14% |
| Elongation | 45 % | 45 % | 0% |
| Elastic modulus | 210,000 MPa | 205,000 MPa | -2% |
| Density | 8,600 kg/m³ | 8,050 kg/m³ | -6% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000014 1/K | +15% |
Difference is ATI 601 (UNS N06601) relative to ATI 59 (UNS N06059). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- N06059
- standard
- ATI Technical Data Sheet
- heat treatment
- Solution Annealed
- grade
- N06601
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed 982C (1800F)
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators