| Property | ATI 22 (UNS N06022) | ATI 59 (UNS N06059) | Difference |
|---|---|---|---|
| Yield strength | 345 MPa | 310 MPa | -10% |
| Tensile strength | 724 MPa | 690 MPa | -5% |
| Elongation | 67 % | 45 % | -33% |
| Elastic modulus | 207,000 MPa | 210,000 MPa | +1% |
| Density | 8,690 kg/m³ | 8,600 kg/m³ | -1% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000012 1/K | -4% |
Difference is ATI 59 (UNS N06059) relative to ATI 22 (UNS N06022). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- N06022
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed
- grade
- N06059
- standard
- ATI Technical Data Sheet
- heat treatment
- Solution Annealed
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators