ATI 22 (UNS N06022) vs ATI 601 (UNS N06601)
Property comparison of ATI 22 (UNS N06022) and ATI 601 (UNS N06601), both nickel alloy.
| Property | ATI 22 (UNS N06022) | ATI 601 (UNS N06601) | Difference |
|---|---|---|---|
| Yield strength | 345 MPa | 440 MPa | +28% |
| Tensile strength | 724 MPa | 790 MPa | +9% |
| Elongation | 67 % | 45 % | -33% |
| Elastic modulus | 207,000 MPa | 205,000 MPa | -1% |
| Density | 8,690 kg/m³ | 8,050 kg/m³ | -7% |
| Thermal conductivity | 9.4 W/m·K | 11.2 W/m·K | +19% |
| Specific heat | 422 J/kg·K | 460 J/kg·K | +9% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000014 1/K | +10% |
Difference is ATI 601 (UNS N06601) relative to ATI 22 (UNS N06022). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- N06022
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed
- grade
- N06601
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed 982C (1800F)
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators