ATI 22 (UNS N06022) vs ATI 520
Property comparison of ATI 22 (UNS N06022) and ATI 520, both nickel alloy.
| Property | ATI 22 (UNS N06022) | ATI 520 | Difference |
|---|---|---|---|
| Yield strength | 345 MPa | 828 MPa | +140% |
| Tensile strength | 724 MPa | 1,310 MPa | +81% |
| Elongation | 67 % | 20 % | -70% |
| Density | 8,690 kg/m³ | 8,220 kg/m³ | -5% |
Difference is ATI 520 relative to ATI 22 (UNS N06022). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
ATI 22 (UNS N06022)
- grade
- N06022
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed
ATI 520
- grade
- Ni-Cr-Co-Mo (N07520)
- standard
- UNS N07520
- heat treatment
- As-specified (bar)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculatorsRelated comparisons
A 286vsATI 22 (UNS N06022)A 286vsATI 520AstroloyvsATI 22 (UNS N06022)AstroloyvsATI 520ATI 10242 (Ni-25Mo-8Cr age-hardenable, low thermal expansion)vsATI 22 (UNS N06022)ATI 10242 (Ni-25Mo-8Cr age-hardenable, low thermal expansion)vsATI 520ATI 22 (UNS N06022)vsATI 59 (UNS N06059)ATI 22 (UNS N06022)vsATI 601 (UNS N06601)