Property comparison of A 286 and ATI 22 (UNS N06022), both nickel alloy.
| Property | A 286 | ATI 22 (UNS N06022) | Difference |
|---|---|---|---|
| Yield strength | 655 MPa | 345 MPa | -47% |
| Tensile strength | 1,000 MPa | 724 MPa | -28% |
| Elongation | 24 % | 67 % | +179% |
| Elastic modulus | 199,000 MPa | 207,000 MPa | +4% |
| Density | 7,916 kg/m³ | 8,690 kg/m³ | +10% |
| Brinell hardness | 304 HB | 172 HB | -43% |
| Thermal conductivity | 12.7 W/m·K | 9.4 W/m·K | -26% |
| Specific heat | 461 J/kg·K | 422 J/kg·K | -8% |
| Coefficient of thermal expansion | 0.000017 1/K | 0.000012 1/K | -25% |
| Melting point | 1,399 °C | 1,371 °C | -2% |
Difference is ATI 22 (UNS N06022) relative to A 286. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
A 286
- grade
- S66286
- standard
- Special Metals / ATI Materials tech bulletin A-286 (UNS S66286); High Temp Metals A-286 tech data sheet
- heat treatment
- solution treat 982C/1h OQ + age 719C/16h AC
ATI 22 (UNS N06022)
- grade
- N06022
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators