Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
A 286 vs Astroloy
Property comparison of A 286 and Astroloy, both nickel alloy.
| Property | A 286 | Astroloy | Difference |
|---|---|---|---|
| Yield strength | 655 MPa | 965 MPa | +47% |
| Tensile strength | 1,000 MPa | 1,275 MPa | +28% |
| Elongation | 24 % | 10 % | -58% |
| Density | 7,916 kg/m³ | 7,920 kg/m³ | 0% |
Difference is Astroloy relative to A 286. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
A 286
- grade
- S66286
- standard
- Special Metals / ATI Materials tech bulletin A-286 (UNS S66286); High Temp Metals A-286 tech data sheet
- heat treatment
- solution treat 982C/1h OQ + age 719C/16h AC
Astroloy
- grade
- Ni-Co-Cr-Mo-Al-Ti (N13017)
- standard
- AMS 5846; EMS 55389
- heat treatment
- Aged (bar)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.