Zircadyne-705-Annealed-316C — Refractory

Category
Refractory
Material Id
Zircadyne 705 Annealed 316C
Cte per K (1/K)
0.000006
Density Kg M3 (kg/m3)
6,640
Elastic Modulus MPa (MPa)
81,000
Elongation Percent (%)
29
Grade
R60705
Heat Treatment
Annealed
Melting Point C (°C)
1,840
Name
Zircadyne 705 (UNS R60705)
Poisson Ratio (dimensionless)
0.33
Property Basis
Typical
Shear Modulus MPa (MPa)
34,500
Specific Heat J kgK (J/(kg·K))
280.5
Standard
ASTM B551 / B523 / B493 / B550 / B658
Tensile Strength MPa (MPa)
299.7
Test Temperature C (C)
316
Thermal Conductivity W mK (W/(m·K))
17.1
Yield Strength MPa (MPa)
190.2

Source: ASTM B551 / B523 / B493 / B550 / B658

refractory — material id Zircadyne_705_Annealed_316C · elastic modulus MPa 81000 MPa · tensile strength MPa 299.7 MPa · yield strength MPa 190.2 MPa · cte per K 5.75e-06 1/K | Metal Alloy Properties | Engineering Database