Zircadyne-702-Annealed-204C — Refractory

Category
Refractory
Material Id
Zircadyne 702 Annealed 204C
Cte per K (1/K)
0.000007
Density Kg M3 (kg/m3)
6,510
Elastic Modulus MPa (MPa)
86,900
Elongation Percent (%)
49
Grade
R60702
Heat Treatment
Annealed
Melting Point C (°C)
1,852
Name
Zircadyne 702 (UNS R60702)
Poisson Ratio (dimensionless)
0.35
Property Basis
Typical
Shear Modulus MPa (MPa)
36,200
Specific Heat J kgK (J/(kg·K))
284.7
Standard
ASTM B551 / B523 / B493 / B550 / B658
Tensile Strength MPa (MPa)
229.6
Test Temperature C (C)
204
Thermal Conductivity W mK (W/(m·K))
22
Yield Strength MPa (MPa)
139.3

Source: ASTM B551 / B523 / B493 / B550 / B658