Ta-2.5W — Refractory
- Category
- Refractory
- Material Id
- Ta 2.5W
- Cte per K (1/K)
- 0.000006
- Density Kg M3 (kg/m3)
- 16,600
- Elastic Modulus MPa (MPa)
- 186,000
- Elongation Percent (%)
- 25
- Grade
- R05252
- Heat Treatment
- Annealed
- Melting Point C (°C)
- 2,996
- Name
- Ta-2.5W (Ta-97.5-W-2.5) Annealed
- Standard
- ASTM B365 R05252 / Plansee Ta Alloy Product Data
- Tensile Strength MPa (MPa)
- 310
- Yield Strength MPa (MPa)
- 207