Zircadyne-702-Annealed-260C — Refractory
- Category
- Refractory
- Material Id
- Zircadyne 702 Annealed 260C
- Cte per K (1/K)
- 0.000007
- Density Kg M3 (kg/m3)
- 6,510
- Elastic Modulus MPa (MPa)
- 80,700
- Elongation Percent (%)
- 49
- Grade
- R60702
- Heat Treatment
- Annealed
- Melting Point C (°C)
- 1,852
- Name
- Zircadyne 702 (UNS R60702)
- Poisson Ratio (dimensionless)
- 0.35
- Property Basis
- Typical
- Shear Modulus MPa (MPa)
- 36,200
- Specific Heat J kgK (J/(kg·K))
- 284.7
- Standard
- ASTM B551 / B523 / B493 / B550 / B658
- Tensile Strength MPa (MPa)
- 200.6
- Test Temperature C (C)
- 260
- Thermal Conductivity W mK (W/(m·K))
- 22
- Yield Strength MPa (MPa)
- 128.9
Source: ASTM B551 / B523 / B493 / B550 / B658