Fatigue Sn Curves: titanium_6Al4V_shot_peened
Fatigue S-N curve data � stress amplitude vs. cycles to failure for various materials, loading types, and surface conditions per ASM Atlas of Fatigue Curves and MMPDS
| material id | cycles | Sut MPa (MPa) | Sut ksi (ksi) | endurance limit MPa (MPa) | endurance limit ksi (ksi) | loading type | stress amplitude MPa (MPa) | stress amplitude ksi (ksi) | stress ratio | surface condition |
|---|---|---|---|---|---|---|---|---|---|---|
| titanium_6Al4V_shot_peened | 1,000 | 950 | 137.8 | 560 | 81.2 | rotating_bending | 890 | 129.1 | -1 | shot_peened |
| titanium_6Al4V_shot_peened | 3,000 | 950 | 137.8 | 560 | 81.2 | rotating_bending | 812 | 117.7 | -1 | shot_peened |
| titanium_6Al4V_shot_peened | 10,000 | 950 | 137.8 | 560 | 81.2 | rotating_bending | 745 | 108 | -1 | shot_peened |
This is a sample. Search the full fatigue sn curves dataset and 300+ more by creating a free account and accessing the database.
Get started for FREERelated data
aluminum_2024_T3_machined3 rowsaluminum_2024_T3_shot_peened3 rowsaluminum_2024_T43 rowsaluminum_6061_T63 rowsaluminum_7075_T63 rowsaluminum_7075_T6_corroded3 rowsaluminum_7075_T6_machined3 rowscast_iron_gray_303 rowscopper_C11000_annealed3 rowsinconel_718_650C3 rowsinconel_718_RT3 rowsstainless_3043 rows