| material id | cycles | Sut MPa (MPa) | Sut ksi (ksi) | endurance limit MPa (MPa) | endurance limit ksi (ksi) | loading type | stress amplitude MPa (MPa) | stress amplitude ksi (ksi) | stress ratio | surface condition |
|---|---|---|---|---|---|---|---|---|---|---|
| aluminum_2024_T3_shot_peened | 1,000 | 483 | 70 | 165 | 23.9 | rotating_bending | 475 | 68.9 | -1 | shot_peened |
| aluminum_2024_T3_shot_peened | 3,000 | 483 | 70 | 165 | 23.9 | rotating_bending | 428 | 62.1 | -1 | shot_peened |
| aluminum_2024_T3_shot_peened | 10,000 | 483 | 70 | 165 | 23.9 | rotating_bending | 378 | 54.8 | -1 | shot_peened |