Fatigue Sn Curves: aluminum_7075_T6_machined
Fatigue S-N curve data � stress amplitude vs. cycles to failure for various materials, loading types, and surface conditions per ASM Atlas of Fatigue Curves and MMPDS
| material id | cycles | Sut MPa (MPa) | Sut ksi (ksi) | endurance limit MPa (MPa) | endurance limit ksi (ksi) | loading type | stress amplitude MPa (MPa) | stress amplitude ksi (ksi) | stress ratio | surface condition |
|---|---|---|---|---|---|---|---|---|---|---|
| aluminum_7075_T6_machined | 1,000 | 572 | 82.9 | 159 | 23.1 | rotating_bending | 514.8 | 74.7 | -1 | machined |
| aluminum_7075_T6_machined | 3,000 | 572 | 82.9 | 159 | 23.1 | rotating_bending | 462 | 67 | -1 | machined |
| aluminum_7075_T6_machined | 10,000 | 572 | 82.9 | 159 | 23.1 | rotating_bending | 402 | 58.3 | -1 | machined |