Fatigue Sn Curves: aluminum_6061_T6
Fatigue S-N curve data � stress amplitude vs. cycles to failure for various materials, loading types, and surface conditions per ASM Atlas of Fatigue Curves and MMPDS
| material id | cycles | Sut MPa (MPa) | Sut ksi (ksi) | endurance limit MPa (MPa) | endurance limit ksi (ksi) | loading type | stress amplitude MPa (MPa) | stress amplitude ksi (ksi) | stress ratio | surface condition |
|---|---|---|---|---|---|---|---|---|---|---|
| aluminum_6061_T6 | 1,000 | 310 | 44.9 | 108.5 | 15.7 | rotating_bending | 279 | 40.5 | -1 | machined |
| aluminum_6061_T6 | 5,000 | 310 | 44.9 | 108.5 | 15.7 | rotating_bending | 237 | 34.4 | -1 | machined |
| aluminum_6061_T6 | 10,000 | 310 | 44.9 | 108.5 | 15.7 | rotating_bending | 218 | 31.6 | -1 | machined |
This is a sample. Search the full fatigue sn curves dataset and 300+ more by creating a free account and accessing the database.
Get started for FREERelated data
aluminum_2024_T3_machined3 rowsaluminum_2024_T3_shot_peened3 rowsaluminum_2024_T43 rowsaluminum_7075_T63 rowsaluminum_7075_T6_corroded3 rowsaluminum_7075_T6_machined3 rowscast_iron_gray_303 rowscopper_C11000_annealed3 rowsinconel_718_650C3 rowsinconel_718_RT3 rowsstainless_3043 rowsstainless_3163 rows