Sample data from Engineering Database — 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Reference Data/Aerospace Materials/CH2 AISI 4135 TUBING QUENCHED and TEMPEREDA 0 5B S 2 3 1 0 C4 C4

Aerospace Materials: CH2 AISI 4135 TUBING QUENCHED and TEMPEREDA 0 5B S 2 3 1 0 C4 C4

Aerospace material mechanical properties and design allowables at ambient, elevated, and cryogenic temperatures per MMPDS-11 (Metallic Materials Properties Development and Standardization). Covers primary structural alloys: aluminum (2024-T3, 7075-T6, 6061-T6, 2219-T87), titanium (Ti-6Al-4V), nickel superalloys (Inconel 718), and steels (300M, 4130, 4340).

Materials Sciencematerial id: CH2 AISI 4135 TUBING QUENCHED and TEMPEREDA 0 5B S 2 3 1 0 C4 C41 row
material idtemp fE Msi (Msi)Ec Msi (Msi)Fbru ksi (ksi)Fbru ksi 2 (ksi)Fbry ksi (ksi)Fbry ksi 2 (ksi)Fcy ksi (ksi)Fsu ksi (ksi)Ftu ksi (ksi)Fty ksi (ksi)G Msi (Msi)basisconditiondensity lb in3 (lb/in^3)designationformpoisson ratiospecificationthickness range
CH2 AISI 4135 TUBING QUENCHED AND TEMPEREDA 0 5B S 2 3 1 0 C4 C470292930838027430218112020016511SQuenched and tempereda0.283AISI 4135Tubing0.32AMS-T-6735< 0.5b