Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Carbon Steel/Steel 12DN2FL GOST 977-88 vs Steel 12MCh GOST 20072-74

Steel 12DN2FL GOST 977-88 vs Steel 12MCh GOST 20072-74

Property comparison of Steel 12DN2FL GOST 977-88 and Steel 12MCh GOST 20072-74, both carbon steel.

Carbon Steel11 compared properties
PropertySteel 12DN2FL GOST 977-88Steel 12MCh GOST 20072-74Difference
Yield strength638 MPa235 MPa-63%
Tensile strength785 MPa410 MPa-48%
Elongation12 %21 %+75%
Elastic modulus200,000 MPa212,000 MPa+6%
Shear modulus77,000 MPa82,000 MPa+6%
Poisson ratio0.30.29-3%
Density7,820 kg/m³7,850 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel 12MCh GOST 20072-74 relative to Steel 12DN2FL GOST 977-88. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel 12DN2FL GOST 977-88
standard
GOST
heat treatment
Quenched and tempered