Carbon Steel11 compared properties
PropertySteel 12DN2FL GOST 977-88Steel 13Ch14N3V2FR GOST 5949-75Difference
Yield strength638 MPa885 MPa+39%
Tensile strength785 MPa1,130 MPa+44%
Elongation12 %12 %0%
Elastic modulus200,000 MPa200,000 MPa0%
Shear modulus77,000 MPa77,000 MPa0%
Poisson ratio0.30.30%
Density7,820 kg/m³7,850 kg/m³0%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel 13Ch14N3V2FR GOST 5949-75 relative to Steel 12DN2FL GOST 977-88. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel 12DN2FL GOST 977-88
standard
GOST
heat treatment
Quenched and tempered
Steel 13Ch14N3V2FR GOST 5949-75
standard
GOST
heat treatment

What else is in Engineering Database

Related comparisons

View each material