Carbon Steel10 compared properties
PropertySteel 12ChN2 GOST 4543-71Steel 12DN2FL GOST 977-88Difference
Yield strength600 MPa638 MPa+6%
Tensile strength800 MPa785 MPa-2%
Elastic modulus211,000 MPa200,000 MPa-5%
Shear modulus82,000 MPa77,000 MPa-6%
Poisson ratio0.290.3+3%
Density7,880 kg/m³7,820 kg/m³-1%
Thermal conductivity51.9 W/m·K51.9 W/m·K0%
Specific heat455 J/kg·K455 J/kg·K0%
Coefficient of thermal expansion0.000012 1/K0.000012 1/K0%
Melting point1,480 °C1,480 °C0%

Difference is Steel 12DN2FL GOST 977-88 relative to Steel 12ChN2 GOST 4543-71. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Steel 12ChN2 GOST 4543-71
standard
GOST
heat treatment
Quenching and cooling in the oil
Steel 12DN2FL GOST 977-88
standard
GOST
heat treatment
Quenched and tempered

What else is in Engineering Database

Related comparisons

View each material