Cobalt Alloy3 compared properties
PropertyMp35nStellite 6 (Co-28Cr-4W-1C) castDifference
Density8,430 kg/m³8,440 kg/m³0%
Coefficient of thermal expansion0.000013 1/K0.000012 1/K-6%
Melting point1,378 °C1,305 °C-5%

Difference is Stellite 6 (Co-28Cr-4W-1C) cast relative to Mp35n. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Mp35n
grade
R30035
standard
SPS Technologies / Carpenter Technology MP35N datasheet (AMS 5844)
heat treatment
cold-worked + aged 566C/4h
Stellite 6 (Co-28Cr-4W-1C) cast
grade
R30006
standard
Kennametal Stellite datasheet (Stellite 6 Alloy Technical Data)
heat treatment
as-cast