Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cobalt Alloy/Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed vs Mp35n

Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed vs Mp35n

Property comparison of Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed and Mp35n, both cobalt alloy.

Cobalt Alloy7 compared properties
PropertyElgiloy (Co-20Cr-15Ni-7Mo-Fe) annealedMp35nDifference
Yield strength310 MPa1,551 MPa+400%
Elastic modulus193,000 MPa232,800 MPa+21%
Poisson ratio0.30.4+33%
Density8,300 kg/m³8,430 kg/m³+2%
Thermal conductivity12.5 W/m·K13.4 W/m·K+7%
Coefficient of thermal expansion0.000015 1/K0.000013 1/K-15%
Melting point1,420 °C1,378 °C-3%

Difference is Mp35n relative to Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Elgiloy (Co-20Cr-15Ni-7Mo-Fe) annealed
grade
R30003
standard
Elgiloy Specialty Metals Wire Data Sheet (ASTM F1058 / AMS 5833)
heat treatment
annealed
Mp35n
grade
R30035
standard
SPS Technologies / Carpenter Technology MP35N datasheet (AMS 5844)
heat treatment
cold-worked + aged 566C/4h