Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Cobalt Alloy/Elgiloy (Co-20Cr-15Ni-7Mo-Fe) full hard vs Stellite 6 (Co-28Cr-4W-1C) cast

Elgiloy (Co-20Cr-15Ni-7Mo-Fe) full hard vs Stellite 6 (Co-28Cr-4W-1C) cast

Property comparison of Elgiloy (Co-20Cr-15Ni-7Mo-Fe) full hard and Stellite 6 (Co-28Cr-4W-1C) cast, both cobalt alloy.

Cobalt Alloy3 compared properties
PropertyElgiloy (Co-20Cr-15Ni-7Mo-Fe) full hardStellite 6 (Co-28Cr-4W-1C) castDifference
Density8,300 kg/m³8,440 kg/m³+2%
Coefficient of thermal expansion0.000015 1/K0.000012 1/K-21%
Melting point1,420 °C1,305 °C-8%

Difference is Stellite 6 (Co-28Cr-4W-1C) cast relative to Elgiloy (Co-20Cr-15Ni-7Mo-Fe) full hard. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Elgiloy (Co-20Cr-15Ni-7Mo-Fe) full hard
grade
R30003
standard
Elgiloy Specialty Metals Wire Data Sheet (ASTM F1058 / AMS 5833)
heat treatment
cold-reduced (full hard)
Stellite 6 (Co-28Cr-4W-1C) cast
grade
R30006
standard
Kennametal Stellite datasheet (Stellite 6 Alloy Technical Data)
heat treatment
as-cast

What else is in Engineering Database