L 605 vs Mp35n
Property comparison of L 605 and Mp35n, both cobalt alloy.
| Property | L 605 | Mp35n | Difference |
|---|---|---|---|
| Yield strength | 450 MPa | 1,551 MPa | +245% |
| Tensile strength | 970 MPa | 1,758 MPa | +81% |
| Elongation | 52 % | 12 % | -77% |
| Elastic modulus | 225,000 MPa | 232,800 MPa | +3% |
| Poisson ratio | 0.29 | 0.4 | +38% |
| Density | 9,130 kg/m³ | 8,430 kg/m³ | -8% |
| Thermal conductivity | 9.4 W/m·K | 13.4 W/m·K | +43% |
| Coefficient of thermal expansion | 0.000012 1/K | 0.000013 1/K | +4% |
| Melting point | 1,370 °C | 1,378 °C | +1% |
Difference is Mp35n relative to L 605. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
L 605
- grade
- R30605
- standard
- Haynes International datasheet H-3000C
- heat treatment
- annealed
Mp35n
- grade
- R30035
- standard
- SPS Technologies / Carpenter Technology MP35N datasheet (AMS 5844)
- heat treatment
- cold-worked + aged 566C/4h
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators