Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Tin Alloy/Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base vs Babbitt Grade 8 (Pb-5Sn-15Sb) lead-base

Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base vs Babbitt Grade 8 (Pb-5Sn-15Sb) lead-base

Property comparison of Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base and Babbitt Grade 8 (Pb-5Sn-15Sb) lead-base, both tin alloy.

Tin Alloy7 compared properties
PropertyBabbitt Grade 7 (Pb-9.3Sn-15Sb) lead-baseBabbitt Grade 8 (Pb-5Sn-15Sb) lead-baseDifference
Yield strength24 MPa18 MPa-25%
Tensile strength72 MPa70 MPa-3%
Elongation4 %5 %+25%
Density10,000 kg/m³10,000 kg/m³0%
Brinell hardness22.5 HB20 HB-11%
Coefficient of thermal expansion0.000026 1/K0.000026 1/K0%
Melting point254 °C255 °C0%

Difference is Babbitt Grade 8 (Pb-5Sn-15Sb) lead-base relative to Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Babbitt Grade 7 (Pb-9.3Sn-15Sb) lead-base
grade
Grade 7 lead-base
standard
ASTM B23
heat treatment
chill cast
Babbitt Grade 8 (Pb-5Sn-15Sb) lead-base
grade
Grade 8 lead-base
standard
ASTM B23
heat treatment
chill cast