Part of Engineering Database. 375 reference tables, deterministic calculators, and Engineering AI. Sign up free
Home/Compare/Nickel Alloy/ATI C-263 (Ni-Co-Cr-Mo precipitation-hardened superalloy, age hardened) vs ATI H-W

ATI C-263 (Ni-Co-Cr-Mo precipitation-hardened superalloy, age hardened) vs ATI H-W

Property comparison of ATI C-263 (Ni-Co-Cr-Mo precipitation-hardened superalloy, age hardened) and ATI H-W, both nickel alloy.

Nickel Alloy4 compared properties
PropertyATI C-263 (Ni-Co-Cr-Mo precipitation-hardened superalloy, age hardened)ATI H-WDifference
Yield strength621 MPa517 MPa-17%
Tensile strength1,034 MPa966 MPa-7%
Elongation35 %50 %+43%
Density8,360 kg/m³8,990 kg/m³+8%

Difference is ATI H-W relative to ATI C-263 (Ni-Co-Cr-Mo precipitation-hardened superalloy, age hardened). Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

ATI C-263 (Ni-Co-Cr-Mo precipitation-hardened superalloy, age hardened)
grade
UNS N07263
standard
ATI Technical Data Sheet
heat treatment
Solution anneal 1038-1177°C + age 802°C/8h AC (AMS 5872E)
ATI H-W
grade
Ni-Mo-Cr (N10004)
standard
UNS N10004
heat treatment
Annealed (bar)