| Property | ATI 520 | ATI 601 (UNS N06601) | Difference |
|---|---|---|---|
| Yield strength | 828 MPa | 440 MPa | -47% |
| Tensile strength | 1,310 MPa | 790 MPa | -40% |
| Elongation | 20 % | 45 % | +125% |
| Density | 8,220 kg/m³ | 8,050 kg/m³ | -2% |
Difference is ATI 601 (UNS N06601) relative to ATI 520. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
ATI 520
- grade
- Ni-Cr-Co-Mo (N07520)
- standard
- UNS N07520
- heat treatment
- As-specified (bar)
ATI 601 (UNS N06601)
- grade
- N06601
- standard
- ATI Technical Data Sheet
- heat treatment
- Annealed 982C (1800F)
What else is in Engineering Database
Iron Engine ↗Engineering AI at ironengine.ai
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculatorsRelated comparisons
A 286vsATI 520A 286vsATI 601 (UNS N06601)AstroloyvsATI 520AstroloyvsATI 601 (UNS N06601)ATI 10242 (Ni-25Mo-8Cr age-hardenable, low thermal expansion)vsATI 520ATI 10242 (Ni-25Mo-8Cr age-hardenable, low thermal expansion)vsATI 601 (UNS N06601)ATI 22 (UNS N06022)vsATI 520ATI 22 (UNS N06022)vsATI 601 (UNS N06601)