Am 355 vs SAE 302 Stainless Steel (25% hard strip)
Property comparison of Am 355 and SAE 302 Stainless Steel (25% hard strip), both stainless steel.
| Property | Am 355 | SAE 302 Stainless Steel (25% hard strip) | Difference |
|---|---|---|---|
| Yield strength | 1,138 MPa | 515 MPa | -55% |
| Tensile strength | 1,379 MPa | 860 MPa | -38% |
| Elongation | 10 % | 12 % | +20% |
| Elastic modulus | 199,948 MPa | 193,000 MPa | -3% |
| Shear modulus | 75,842 MPa | 74,231 MPa | -2% |
| Poisson ratio | 0.32 | 0.3 | -6% |
| Density | 7,806 kg/m³ | 7,850 kg/m³ | +1% |
Difference is SAE 302 Stainless Steel (25% hard strip) relative to Am 355. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- AM-355
- standard
- MIL-HDBK-5J
- heat treatment
- SCT850
- grade
- 302
- standard
- SAE
- heat treatment
- 25% hard strip
About 300-series stainless steels
Austenitic stainless steels gain corrosion resistance from chromium and nickel and are non-magnetic in the annealed condition. 304 covers most general-purpose work; 316 adds molybdenum for chloride and seawater service. They cannot be hardened by heat treatment and rely on cold work for higher strength.
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators