PropertyAm 350Am 355Difference
Yield strength1,014 MPa1,138 MPa+12%
Tensile strength1,262 MPa1,379 MPa+9%
Elastic modulus199,948 MPa199,948 MPa0%
Shear modulus75,842 MPa75,842 MPa0%
Poisson ratio0.320.320%
Density7,806 kg/m³7,806 kg/m³0%

Difference is Am 355 relative to Am 350. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.

Identification

Am 350
grade
AM-350
standard
MIL-HDBK-5J
heat treatment
SCT 850
Am 355
grade
AM-355
standard
MIL-HDBK-5J
heat treatment
SCT850

About 300-series stainless steels

Austenitic stainless steels gain corrosion resistance from chromium and nickel and are non-magnetic in the annealed condition. 304 covers most general-purpose work; 316 adds molybdenum for chloride and seawater service. They cannot be hardened by heat treatment and rely on cold work for higher strength.

What else is in Engineering Database

Related comparisons

View each material