| Property | AISI 301 | Am 355 | Difference |
|---|---|---|---|
| Yield strength | 455.1 MPa | 1,138 MPa | +150% |
| Tensile strength | 503.3 MPa | 1,379 MPa | +174% |
| Elastic modulus | 199,948 MPa | 199,948 MPa | 0% |
| Shear modulus | 77,221 MPa | 75,842 MPa | -2% |
| Density | 7,916 kg/m³ | 7,806 kg/m³ | -1% |
Difference is Am 355 relative to AISI 301. Values are taken from the representative row of each material; both materials may have multiple heat treatments or conditions on their individual pages.
Identification
- grade
- AISI 301
- standard
- MIL-HDBK-5J
- heat treatment
- 1/4 Hard
- grade
- AM-355
- standard
- MIL-HDBK-5J
- heat treatment
- SCT850
About 300-series stainless steels
Austenitic stainless steels gain corrosion resistance from chromium and nickel and are non-magnetic in the annealed condition. 304 covers most general-purpose work; 316 adds molybdenum for chloride and seawater service. They cannot be hardened by heat treatment and rely on cold work for higher strength.
What else is in Engineering Database
AI built for engineering. Searches the engineering database, performs calculations, gives source-backed engineering insights.
Get started for free ↗Reference Data375 engineering tablesMaterial properties, pipe and shape dimensions, code tables, and electrical ratings across mechanical, civil, chemical, electrical, materials, and manufacturing engineering.
Browse dataCalculatorsDeterministic engineering calculatorsSizing, checking, and conversion tools that run against the reference tables. Inputs are code-compliant, outputs are traceable to the source standard.
Browse calculators